General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 18 g/cm³ Show Supplier Material materials with Densidad of 18 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 360 GPa Show Supplier Material materials with Módulo elástico of 360 GPa |
Chemical properties
Property | Value |
---|---|
Cobre | binder |
Níquel | binder |
Wolframio | 95 % Show Supplier Material materials with Wolframio of 95 % |
Technological properties
Property | ||
---|---|---|
Application areas | Inermet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Paramagnetic |