General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 16.6 g/cm³ Show Supplier Material materials with Densidad of 16.6 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 4 - 10 mm Show Supplier Material materials with Diámetro of 4 - 10 mm |
Longitud | 300 - 2500 mm Show Supplier Material materials with Longitud of 300 - 2500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 4 x 500-2000 ; 6 x 500-2500 ; 10 x 300-2500 |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % |
Límite elástico Rp 0,2 | 23.0 °C | 103 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 103 MPa |
Resistencia a la tracción | 23.0 °C | 172 MPa Show Supplier Material materials with Resistencia a la tracción of 172 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de cristalización | 900 - 1450 °C Show Supplier Material materials with Temperatura de cristalización of 900 - 1450 °C |
Temperatura de fusión | 2966 °C Show Supplier Material materials with Temperatura de fusión of 2966 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.3 eV Show Supplier Material materials with Función de trabajo of 4.3 eV |
Temperatura de transición de los superconductores | -268.65 °C Show Supplier Material materials with Temperatura de transición de los superconductores of -268.65 °C |
Acústico
Chemical properties
Property | Value | Comment |
---|---|---|
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % | |
Carbono | 1E-3 % Show Supplier Material materials with Carbono of 1E-3 % | |
Hidrógeno | 4E-4 % Show Supplier Material materials with Hidrógeno of 4E-4 % | |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % | |
Molibdeno | 1E-3 % Show Supplier Material materials with Molibdeno of 1E-3 % | |
Niobio | 1.9E-3 % Show Supplier Material materials with Niobio of 1.9E-3 % | |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % | |
Níquel | 5E-4 % Show Supplier Material materials with Níquel of 5E-4 % | |
Oxígeno | 1.3E-3 % Show Supplier Material materials with Oxígeno of 1.3E-3 % | |
Silicona | 1E-3 % Show Supplier Material materials with Silicona of 1E-3 % | |
Titanio | 1E-4 % Show Supplier Material materials with Titanio of 1E-4 % | |
Tántalo | 99.95 % Show Supplier Material materials with Tántalo of 99.95 % | min |
Wolframio | 2E-3 % Show Supplier Material materials with Wolframio of 2E-3 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Outstanding resistance against aqueous solutions and metal melts. | |
Other | This material has excellent cold ductility, superconductivity and a high level of biocompatibility. |