General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 10.15 g/cm³ Show Supplier Material materials with Densidad of 10.15 g/cm³ |
Rugosidad superficial | 0.8 - 1 μm Show Supplier Material materials with Rugosidad superficial of 0.8 - 1 μm |
Medidas
Property | Value |
---|---|
Diámetro | 2 - 30 mm Show Supplier Material materials with Diámetro of 2 - 30 mm |
Longitud | 100 - 3000 mm Show Supplier Material materials with Longitud of 100 - 3000 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 2 x 300-3000; 3 x 300-3000; 4 x 300-3000; 4.75 x 300-3000; 5 x 300-3000; 6 x 300-3000; 6.35 x 300-3000; 7 x 300-2900; 8 x 300-2900; 9 x 300-2900; 9.525 x 300-1400; 10 x 100-2900; 12 x 100-2900; 12.7 x 100-1200; 13 x 100-1900; 14 x 100-2000; 15 x 100-1900; 15.875 x 100-2000; 19.05 x 100-1800; 20 x 100-2100; 22.225 x 100-1700; 25 x 100-2100; 30 x 100-1900 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 23.0 °C | 215 - 280 [-] Show Supplier Material materials with Dureza Vickers 10 of 215 - 280 [-] |
Elongación | 23.0 °C | 10 - 18 % Show Supplier Material materials with Elongación of 10 - 18 % |
Límite elástico Rp 0,2 | 23.0 °C | 380 - 515 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 380 - 515 MPa |
Resistencia a la tracción | 23.0 °C | 515 - 620 MPa Show Supplier Material materials with Resistencia a la tracción of 515 - 620 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2620 °C Show Supplier Material materials with Temperatura de fusión of 2620 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.39 eV Show Supplier Material materials with Función de trabajo of 4.39 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | 99.97 % Show Supplier Material materials with Molibdeno of 99.97 % |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 6E-4 % Show Supplier Material materials with Oxígeno of 6E-4 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |