General
Medidas
Property | Value |
---|---|
Diámetro | 140 - 165 mm Show Supplier Material materials with Diámetro of 140 - 165 mm |
Longitud | 100 - 500 mm Show Supplier Material materials with Longitud of 100 - 500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 140 x 100-500; 165 x 100-500 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 23.0 °C | 180 - 240 [-] Show Supplier Material materials with Dureza Vickers 10 of 180 - 240 [-] |
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % |
Límite elástico Rp 0,2 | 23.0 °C | 380 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 380 MPa |
Resistencia a la tracción | 23.0 °C | 450 MPa Show Supplier Material materials with Resistencia a la tracción of 450 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2620 °C Show Supplier Material materials with Temperatura de fusión of 2620 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.39 eV Show Supplier Material materials with Función de trabajo of 4.39 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | 99.97 % Show Supplier Material materials with Molibdeno of 99.97 % |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 6E-4 % Show Supplier Material materials with Oxígeno of 6E-4 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |