General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Densidad of 10.2 g/cm³ |
Rugosidad superficial | 1 μm Show Supplier Material materials with Rugosidad superficial of 1 μm |
Medidas
Property | Value |
---|---|
Ancho | 609 - 1550 mm Show Supplier Material materials with Ancho of 609 - 1550 mm |
Espesor | 0.13 - 40 mm Show Supplier Material materials with Espesor of 0.13 - 40 mm |
Longitud | 1300 - 10500 mm Show Supplier Material materials with Longitud of 1300 - 10500 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 1400 x 1550 x 4; 1550 x 2300 x 5; 1550 x 1600 x 7; 1300 x 1650 x 8; 1000 x 1750 x 10; 1200 x 2600 x 12.7; 1200 x 1980 x 16; 1200 x 1530 x 20; 1050 x 1850 x 30; 1050 x 1300 x 40; 609.6 x 1981.2 x 0.127; 609.6 x 9500 x 0.127; 914.4 x 9700 x 0.254; 609.6 x 10200 x 0.254; 609.6 x 1981.2 x 0.254; 609.6 x 10500 x 0.381; 609.6 x 1981.2 x 0.381; 609.6 x 1981.2 x 0.508; 750 x 2000 x 1; 750 x 2300 x 1.5; 750 x 2000 x 2; 750 x 2000 x 2.5; 750 x 1600 x 3 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 220 - 280 [-] Show Supplier Material materials with Dureza Vickers of 220 - 280 [-] |
Elongación | 23.0 °C | 1 - 15 % Show Supplier Material materials with Elongación of 1 - 15 % |
Resistencia a la tracción | 23.0 °C | 640 MPa Show Supplier Material materials with Resistencia a la tracción of 640 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2620 °C Show Supplier Material materials with Temperatura de fusión of 2620 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.39 eV Show Supplier Material materials with Función de trabajo of 4.39 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | 99.97 % Show Supplier Material materials with Molibdeno of 99.97 % |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 6E-4 % Show Supplier Material materials with Oxígeno of 6E-4 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |