General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Densidad of 10.2 g/cm³ |
Rugosidad superficial | 0.2 μm Show Supplier Material materials with Rugosidad superficial of 0.2 μm |
Medidas
Property | Value |
---|---|
Ancho | 600 mm Show Supplier Material materials with Ancho of 600 mm |
Espesor | 0.15 - 1 mm Show Supplier Material materials with Espesor of 0.15 - 1 mm |
Longitud | 2000 mm Show Supplier Material materials with Longitud of 2000 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 600 x 2000 x 0.15; 600 x 2000 x 0.2; 600 x 2000 x 0.25; 600 x 2000 x 0.3; 600 x 2000 x 0.4; 600 x 2000 x 0.5; 600 x 2000 x 1 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 240 - 280 [-] Show Supplier Material materials with Dureza Vickers of 240 - 280 [-] |
Elongación | 23.0 °C | 2 - 10 % Show Supplier Material materials with Elongación of 2 - 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 590 - 620 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 590 - 620 MPa |
Resistencia a la tracción | 23.0 °C | 680 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 680 - 700 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2620 °C Show Supplier Material materials with Temperatura de fusión of 2620 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.39 eV Show Supplier Material materials with Función de trabajo of 4.39 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | 99.97 % Show Supplier Material materials with Molibdeno of 99.97 % |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 6E-4 % Show Supplier Material materials with Oxígeno of 6E-4 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |