General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Densidad of 10.2 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 2 - 3 mm Show Supplier Material materials with Diámetro of 2 - 3 mm |
Dimensions | Available diameters (mm): 2; 2.5; 3 |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Resistencia a la tracción | 23.0 °C | 650 - 1000 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 1000 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2620 °C Show Supplier Material materials with Temperatura de fusión of 2620 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.39 eV Show Supplier Material materials with Función de trabajo of 4.39 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | 99.97 % Show Supplier Material materials with Molibdeno of 99.97 % |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 6E-4 % Show Supplier Material materials with Oxígeno of 6E-4 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Molybdenum-wire is used in a wide variety of high temperature applications. Typical applications are the lighting industry, conductor elements and fabric components in furnace construction and special applications. |