General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Densidad of 10.1 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 76.2 - 127 mm Show Supplier Material materials with Ancho of 76.2 - 127 mm |
Espesor | 0.64 - 0.76 mm Show Supplier Material materials with Espesor of 0.64 - 0.76 mm |
Dimensions | Available dimensions (width x thickness, mm x mm): 76.2 x 0.635; 101.6 x 0.635; 127 x 0.635; 76.2 x 0.762; 101.6 x 0.762; 127 x 0.762 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 250 [-] Show Supplier Material materials with Dureza Vickers of 250 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % | ||
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % | ||
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % | ||
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % | ||
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % | ||
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % | ||
Lantano | 0.52 - 0.62 % Show Supplier Material materials with Lantano of 0.52 - 0.62 % | as La | |
Molibdeno | balance | ||
Nitrógeno | 1E-4 % Show Supplier Material materials with Nitrógeno of 1E-4 % | ||
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % | ||
Otro | 0.61 - 0.73 % Show Supplier Material materials with Otro of 0.61 - 0.73 % | as La₂O₃ | |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % | ||
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % | ||
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | This alloy is mostly machined to produce furnace components such as stranded and other wires, sintering and annealing boats or evaporator coils. In the lighting industry, molybdenum-lanthanum oxide is used, for example, for retaining and feed wires. |