General
Property | Value |
---|---|
Estructura de grano | Fine-grained, homogeneous |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.34E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.34E-6 1/K |
Conductividad térmica | 23.0 °C | 97 W/(m·K) Show Supplier Material materials with Conductividad térmica of 97 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.30E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.30E+7 S/m |
Chemical properties
Property | Value |
---|---|
Molibdeno | balance |
Tántalo | 10.75 % Show Supplier Material materials with Tántalo of 10.75 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thanks to its good adherence to glass and a high level of electrical conductivity, molybdenum is a popular material for electrode layers in thin-film transistors (TFT-LCD) and touch sensors (touch panels). |