General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Densidad of 10.1 g/cm³ |
Rugosidad superficial | 0.15 μm Show Supplier Material materials with Rugosidad superficial of 0.15 μm |
Medidas
Property | Value |
---|---|
Ancho | 1.5 - 10 mm Show Supplier Material materials with Ancho of 1.5 - 10 mm |
Espesor | 0.02 - 0.04 mm Show Supplier Material materials with Espesor of 0.02 - 0.04 mm |
Dimensions | Available dimensions (width x thickness, mm x mm): 1.5 x 0.02; 2 x 0.025; 3 x 0.025; 4 x 0.025; 2 x 0.028; 2.5 x 0.028; 3 x 0.028; 4 x 0.028; 3 x 0.03; 4.8 x 0.033; 5 x 0.035; 6 x 0.035; 10 x 0.04 |
Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia a la tracción | 23.0 °C | 750 - 1000 MPa Show Supplier Material materials with Resistencia a la tracción of 750 - 1000 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % | ||
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % | ||
Carbono | 1.3E-3 % Show Supplier Material materials with Carbono of 1.3E-3 % | ||
Cerio | 0.08 % Show Supplier Material materials with Cerio of 0.08 % | as CeO₂ | |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % | ||
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % | ||
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % | ||
Itrio | 0.47 - 0.6 % Show Supplier Material materials with Itrio of 0.47 - 0.6 % | as Y-mixed oxide | |
Molibdeno | balance | ||
Nitrógeno | 1E-4 % Show Supplier Material materials with Nitrógeno of 1E-4 % | ||
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % | ||
Potasio | 4E-4 % Show Supplier Material materials with Potasio of 4E-4 % | ||
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % | ||
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | MY is primarily used in conductive ESS ribbons and in evaporation boats for applications in the field of coating technology and in the lighting industry. | |
Other | ESS (Elliptically Shaped for Sealing-in) Ribbon with tapered edges by etching. |