Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Tantalum Tungsten Alloy (Ta10W)
Tantalum-Tungsten (TaW) excels due to its good mechanical properties and excellent corrosion resistance. Between 2.5 and 10 percent by weight of tungsten are added to pure tantalum. Although the resulting alloy is up to 1.4 times stronger than pure tantalum, it remains easy to work at temperatures of up to 1600 °C.
Los datos sobre este material han sido proporcionados por Plansee.
All categories
Base plates for semiconductors
Components for epitaxial growth processes
Cylinders for hot isostatic pressing (HIP)
Electrodes for resistance welding made of tungsten and molybdenum
Heating elements for MOCVD
Lead replacement for X-ray shielding
Molybdenum sputtering targets
Nozzles for the production of wool and fibers
Plansee’s newly patented coating material pushing boundaries in sputtering target efficiency
Tungsten Alloy Balancing Weights
Tungsten, molybdenum and tantalum for evaporation coils
Chemical properties
Property | Value |
---|---|
Tántalo | balance |
Wolframio | 10 % Show Supplier Material materials with Wolframio of 10 % |
Technological properties
Property | ||
---|---|---|
Application areas | TaW is specially well suited for the heat exchangers and heating elements used in the chemical equipment construction field. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.