General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10 - 10.15 g/cm³ Show Supplier Material materials with Densidad of 10 - 10.15 g/cm³ |
Rugosidad superficial | 1 μm Show Supplier Material materials with Rugosidad superficial of 1 μm |
Medidas
Property | Value |
---|---|
Diámetro | 16 - 90 mm Show Supplier Material materials with Diámetro of 16 - 90 mm |
Longitud | 100 - 3000 mm Show Supplier Material materials with Longitud of 100 - 3000 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 16 x 100-1500; 18 x 100-2000; 20 x 100-2400; 22.225 x 100-2000; 25 x 100-2200; 26.67 x 100-1700; 30 x 100-1700; 31.75 x 100-1500; 35 x 100-2600; 40 x 100-3000; 45 x 100-2000; 49.5 x 100-2300; 55 x 100-1800; 63.5 x 100-1300; 70 x 100-1800; 80 x 100-1300; 90 x 100-2400 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 235 - 320 [-] Show Supplier Material materials with Dureza Vickers of 235 - 320 [-] |
Elongación | 23.0 °C | 5 - 18 % Show Supplier Material materials with Elongación of 5 - 18 % |
Límite elástico Rp 0,2 | 23.0 °C | 515 - 690 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 515 - 690 MPa |
Resistencia a la tracción | 23.0 °C | 585 - 790 MPa Show Supplier Material materials with Resistencia a la tracción of 585 - 790 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Circonio | 0.06 - 0.12 % Show Supplier Material materials with Circonio of 0.06 - 0.12 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | balance |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 0.01 % Show Supplier Material materials with Oxígeno of 0.01 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Titanio | 0.4 - 0.55 % Show Supplier Material materials with Titanio of 0.4 - 0.55 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C. |