General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Densidad of 10.1 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 400 mm Show Supplier Material materials with Ancho of 400 mm |
Espesor | 10 - 20 mm Show Supplier Material materials with Espesor of 10 - 20 mm |
Longitud | 600 mm Show Supplier Material materials with Longitud of 600 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 400 x 600 x 10; 400 x 600 x 20 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 220 - 320 [-] Show Supplier Material materials with Dureza Vickers of 220 - 320 [-] |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 600 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 600 MPa |
Resistencia a la tracción | 23.0 °C | 650 MPa Show Supplier Material materials with Resistencia a la tracción of 650 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Circonio | 0.06 - 0.12 % Show Supplier Material materials with Circonio of 0.06 - 0.12 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | balance |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 0.01 % Show Supplier Material materials with Oxígeno of 0.01 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Titanio | 0.4 - 0.55 % Show Supplier Material materials with Titanio of 0.4 - 0.55 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C. |