General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 19.2 g/cm³ Show Supplier Material materials with Densidad of 19.2 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 200 - 508 mm Show Supplier Material materials with Ancho of 200 - 508 mm |
Espesor | 0.1 - 0.3 mm Show Supplier Material materials with Espesor of 0.1 - 0.3 mm |
Longitud | 838 - 1000 mm Show Supplier Material materials with Longitud of 838 - 1000 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 200 x 1000 x 0.1; 508 x 838.2 x 0.127; 200 x 1000 x 0.2; 508 x 838.2 x 0.254; 200 x 1000 x 0.3 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 500 - 550 [-] Show Supplier Material materials with Dureza Vickers of 500 - 550 [-] |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 3420 °C Show Supplier Material materials with Temperatura de fusión of 3420 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.54 eV Show Supplier Material materials with Función de trabajo of 4.54 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 6E-4 % Show Supplier Material materials with Carbono of 6E-4 % |
Cobre | 1E-4 % Show Supplier Material materials with Cobre of 1E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 8E-4 % Show Supplier Material materials with Hierro of 8E-4 % |
Molibdeno | 1.2E-3 % Show Supplier Material materials with Molibdeno of 1.2E-3 % |
Níquel | 2E-4 % Show Supplier Material materials with Níquel of 2E-4 % |
Oxígeno | 2E-4 % Show Supplier Material materials with Oxígeno of 2E-4 % |
Plomo | 1E-4 % Show Supplier Material materials with Plomo of 1E-4 % |
Potasio | 1E-4 % Show Supplier Material materials with Potasio of 1E-4 % |
Silicona | 1E-4 % Show Supplier Material materials with Silicona of 1E-4 % |
Wolframio | 99.97 % Show Supplier Material materials with Wolframio of 99.97 % |
Technological properties
Property | ||
---|---|---|
Application areas | Premium Quality sheets are used for many applications where superior finish is desired. It is ideal for deep drawing. |