Wrought Copper High Copper Alloy
ASTM B251 Grade C17000 TD04Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TF00Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TB00Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TH04Aleación de níquel-hierro
EFI Alloy 50 Round BarAleación de hierro
Invar® 36 Free-Machined Round BarAcero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedNickel Chromium Molybdenum Steel
Carbodur 6587 Blank HardenedSuministrada por:
Deutsche Edelstahlwerke (DEW)Wrought Copper High Copper Alloy
ASTM B197 Grade C17300 TH04