Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Tungsten Potassium Alloy (WK65)
Tungsten is doped with 60 to 65 ppm potassium and the material is formed to create wire products with an elongated stacked microstructure. This microstructure gives the material excellent high-temperature properties such as good creep resistance and dimensional stability. Special production steps can be used to make WK65 more load-resistant than WVM.
Los datos sobre este material han sido proporcionados por Plansee.
All categories
Base plates for semiconductors
Components for epitaxial growth processes
Cylinders for hot isostatic pressing (HIP)
Electrodes for resistance welding made of tungsten and molybdenum
Heating elements for MOCVD
Lead replacement for X-ray shielding
Molybdenum sputtering targets
Nozzles for the production of wool and fibers
Plansee’s newly patented coating material pushing boundaries in sputtering target efficiency
Tungsten Alloy Balancing Weights
Tungsten, molybdenum and tantalum for evaporation coils
Chemical properties
Property | Value |
---|---|
Potasio | 6E-4 - 6.5E-4 % Show Supplier Material materials with Potasio of 6E-4 - 6.5E-4 % |
Wolframio | balance |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.