General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 15.5 g/cm³ Show Supplier Material materials with Densidad of 15.5 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 22.0 °C | 8.3E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.3E-6 1/K |
Conductividad térmica | 23.0 °C | 235 W/(m·K) Show Supplier Material materials with Conductividad térmica of 235 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Cobre | balance |
Wolframio | 20 % Show Supplier Material materials with Wolframio of 20 % |
Technological properties
Property | ||
---|---|---|
Application areas | WCu is used for the construction of high-voltage circuit breakers (marketed under the name Elmet®) and for erosion electrodes (marketed under the name Sparkal®). WCu composites are also used as base plates and heat spreaders in radar technology, optoelectronics and high frequency electronics. |