General
Property | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Absorción de agua | 0.7 % Show Supplier Material materials with Absorción de agua of 0.7 % | 2 mm | ISO 62 | 24h immersion at 23°C | |
1.9 % Show Supplier Material materials with Absorción de agua of 1.9 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2.9 % Show Supplier Material materials with Elongación of 2.9 % | dry | ISO 527-2/1A | 5mm/min | |
3.5 % Show Supplier Material materials with Elongación of 3.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 6.1 GPa Show Supplier Material materials with Módulo de flexión of 6.1 GPa | 50%RH | ISO 178 | 2mm/min | |
7.9 GPa Show Supplier Material materials with Módulo de flexión of 7.9 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 7.9 GPa Show Supplier Material materials with Módulo elástico of 7.9 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 200 MPa Show Supplier Material materials with Resistencia a la flexión of 200 MPa | 50%RH | ISO 178 | 2mm/min | |
230 MPa Show Supplier Material materials with Resistencia a la flexión of 230 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 66 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 66 kJ/m² | dry | ISO 179/1eU | 23°C | |
70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | 50%RH | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-05 1/K | ISO 11359-1/-2 | 23°C-55°C |
0.00012 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00012 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |
Temperatura de fusión | 212 °C Show Supplier Material materials with Temperatura de fusión of 212 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.7 % Show Supplier Material materials with Contracción of 0.7 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, Drinking Water, RoHS 2011/65/UE | |
Color | Black | |
Features | Hydrolysis Resistance | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |