General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 6.4 % Show Supplier Material materials with Absorción de agua of 6.4 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-2/1A | 5mm/min | |
7 % Show Supplier Material materials with Elongación of 7 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 6.8 GPa Show Supplier Material materials with Módulo de flexión of 6.8 GPa | 50%RH | ISO 178 | 2mm/min | |
10.1 GPa Show Supplier Material materials with Módulo de flexión of 10.1 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 175 MPa Show Supplier Material materials with Resistencia a la flexión of 175 MPa | 50%RH | ISO 178 | 2mm/min | |
275 MPa Show Supplier Material materials with Resistencia a la flexión of 275 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU | 23°C | |
100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | 50%RH | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | ISO 75/2Af | 1.80 MPa | ||
215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | ISO 75/2Bf | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 210 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 210 °C | ISO 306 | 50°C/h 50N | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | 280/80/30* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | 280/80/30* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 35% Glass Fiber | |
Processing methods | Injection Molding |