General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 5.2 % Show Supplier Material materials with Absorción de agua of 5.2 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.42 g/cm³ Show Supplier Material materials with Densidad of 1.42 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-2/1A | 5mm/min | |
4.5 % Show Supplier Material materials with Elongación of 4.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 6.3 GPa Show Supplier Material materials with Módulo de flexión of 6.3 GPa | 50%RH | ISO 178 | 2mm/min | |
9.9 GPa Show Supplier Material materials with Módulo de flexión of 9.9 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 7.2 GPa Show Supplier Material materials with Módulo elástico of 7.2 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
10.6 GPa Show Supplier Material materials with Módulo elástico of 10.6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 140 MPa Show Supplier Material materials with Resistencia a la flexión of 140 MPa | 50%RH | ISO 178 | 2mm/min | |
220 MPa Show Supplier Material materials with Resistencia a la flexión of 220 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
137 MPa Show Supplier Material materials with Resistencia a la tracción of 137 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | 50%RH | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | 1 mm, 2 mm | IEC 60695-2-12 | ||||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | 1 mm | IEC 60695-2-13 | ||||
775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | 2 mm | IEC 60695-2-13 | |||||
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | ISO 75/2Af | 1.80 MPa | ||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 210 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 210 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | 270/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | 270/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Black | |
Features | Flame Retardant, Halogen-free, Phosphorus-free, Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Other | Federal Motor Vehicle Safety Standards (FMVSS) : Standard-ISO 3795, Assessment-DNI | |
Processing methods | Injection Molding |