General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 2.2 % Show Supplier Material materials with Absorción de agua of 2.2 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1 % Show Supplier Material materials with Moisture absorption of 1 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-2/1A | 5mm/min | |
6 % Show Supplier Material materials with Elongación of 6 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 5.9 GPa Show Supplier Material materials with Módulo de flexión of 5.9 GPa | 50%RH | ISO 178 | 2mm/min | |
7.6 GPa Show Supplier Material materials with Módulo de flexión of 7.6 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 6.8 GPa Show Supplier Material materials with Módulo elástico of 6.8 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 190 MPa Show Supplier Material materials with Resistencia a la flexión of 190 MPa | 50%RH | ISO 178 | 2mm/min | |
235 MPa Show Supplier Material materials with Resistencia a la flexión of 235 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 17 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 17 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | dry | ISO 179/1eU | |
23 °C | 105 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 105 kJ/m² | 50%RH | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | ISO 75/2Af | 1.80 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |