General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Abrasion resistance | 26 mm³ Show Supplier Material materials with Abrasion resistance of 26 mm³ | ISO 4649 | |
Absorción de agua | 0.73 % Show Supplier Material materials with Absorción de agua of 0.73 % | ISO 62@1 | immersion at 23°C |
Densidad | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | ISO 1183 |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dureza Shore D | 35 [-] Show Supplier Material materials with Dureza Shore D of 35 [-] | ISO 7619-1 | 15s |
39 [-] Show Supplier Material materials with Dureza Shore D of 39 [-] | ISO 7619-1 | inst. | |
Elongación | 800 % Show Supplier Material materials with Elongación of 800 % | ISO 527-2/1A | 50mm/min | nominal |
Modulus at 10% elongation | 0.004 GPa Show Supplier Material materials with Modulus at 10% elongation of 0.004 GPa | ISO 527-2/1A | |
Módulo a elongación del 300 % | 0.009 GPa Show Supplier Material materials with Módulo a elongación del 300 % of 0.009 GPa | ISO 527-2/1A | |
Módulo al 100 % de elongación | 0.008 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.008 GPa | ISO 527-2/1A | |
Módulo de flexión | 0.055 GPa Show Supplier Material materials with Módulo de flexión of 0.055 GPa | ISO 178 | 2mm/min |
Módulo elástico | 0.035 GPa Show Supplier Material materials with Módulo elástico of 0.035 GPa | ISO 527-2/1A | 1mm/min |
Resistencia a desgarros | 113 kN/m Show Supplier Material materials with Resistencia a desgarros of 113 kN/m | ISO 34-1 | |
Resistencia a la flexión | 5 MPa Show Supplier Material materials with Resistencia a la flexión of 5 MPa | ISO 178 | 2mm/min |
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 65 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65 °C | ISO 75/2Bf | 0.45 MPa |
Temperatura de fusión | 177 °C Show Supplier Material materials with Temperatura de fusión of 177 °C | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 130 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 130 °C | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 33 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 33 g/10min | ISO 1133 | 230°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |