General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 5.5 % Show Supplier Material materials with Absorción de agua of 5.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.34 g/cm³ Show Supplier Material materials with Densidad of 1.34 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 5.9 GPa Show Supplier Material materials with Módulo de flexión of 5.9 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 6.5 GPa Show Supplier Material materials with Módulo elástico of 6.5 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 170 MPa Show Supplier Material materials with Resistencia a la flexión of 170 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 6.9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.9 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 52 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 52 kJ/m² | dry | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30 °C | 5.2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5.2 kJ/m² | dry | ISO 180/1A | |
23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | dry | ISO 180/1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Thickness | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.7e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.7e-05 1/K | ISO 11359-1/-2 | 23°C-55°C | ||||
0.000206 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000206 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | IEC 60695-2-12 | 1 mm | ||||
Temperatura de flexión bajo carga | 215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | ISO 75/2Af | 1.80 MPa | ||||
250 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 250 °C | ISO 75/2Bf | 0.45 MPa | |||||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 220 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 220 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8 and 1.6, Class: V-0, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+11 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.9 % Show Supplier Material materials with Contracción of 0.9 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.2 % Show Supplier Material materials with Contracción of 1.2 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Velocidad de flujo de la masa derretida | 32 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 32 g/10min | ISO 1133 | 275°C/3.25Kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Flame Retardant, Halogen-free | |
Fillers | 15% Glass Fiber | |
Processing methods | Injection Molding |