General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.44 g/cm³ Show Supplier Material materials with Densidad of 1.44 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | ISO 178 | 2mm/min | |
Módulo elástico | 2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | 2mm/min | |
Resistencia a la tracción | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 2.8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.8 kJ/m² | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.9 % Show Supplier Material materials with Contracción of 1.9 % | 260/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.9 % Show Supplier Material materials with Contracción of 1.9 % | 260/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Black | |
Features | Flame Retardant, Heat Stabilized | |
Processing methods | Injection Molding |