General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.42 g/cm³ Show Supplier Material materials with Densidad of 1.42 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3.8 % Show Supplier Material materials with Elongación of 3.8 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 10.6 GPa Show Supplier Material materials with Módulo elástico of 10.6 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 235 MPa Show Supplier Material materials with Resistencia a la flexión of 235 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | 1 mm, 2 mm | IEC 60695-2-12 | ||||
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | ISO 75/2Af | 1.80 MPa | ||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Rigidez dieléctrica | 44 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 44 kV/mm | 50%RH | IEC 60243-1 | |
45 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 45 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Flame Retardant, Phosphorus-free, Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |