General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 8.4 % Show Supplier Material materials with Absorción de agua of 8.4 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 40 % Show Supplier Material materials with Elongación of 40 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
50 % Show Supplier Material materials with Elongación of 50 % | 50%RH | ISO 527-2/1A | 50mm/min | nominal | ||
Elongation at yield | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | dry | ISO 527-2/1A | 50mm/min | |
25 % Show Supplier Material materials with Elongation at yield of 25 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Límite elástico | 60 MPa Show Supplier Material materials with Límite elástico of 60 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
85 MPa Show Supplier Material materials with Límite elástico of 85 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 2.9 GPa Show Supplier Material materials with Módulo de flexión of 2.9 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 110 MPa Show Supplier Material materials with Resistencia a la flexión of 110 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | 50%RH | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 750 °C Show Supplier Material materials with Glow Wire Flammability Index of 750 °C | 2 mm | IEC 60695-2-12 | ||||
Temperatura de flexión bajo carga | 75 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 75 °C | ISO 75/2Af | 1.80 MPa | ||||
195 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 195 °C | ISO 75/2Bf | 0.45 MPa | |||||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 240 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 240 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.1 % Show Supplier Material materials with Contracción of 1.1 % | 290/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | 290/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Viscosity number | 260 cm³/gr Show Supplier Material materials with Viscosity number of 260 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |