General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-2/1A | 5mm/min | |
25 % Show Supplier Material materials with Elongación of 25 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | 50%RH | ISO 178 | 2mm/min | |
6.7 GPa Show Supplier Material materials with Módulo de flexión of 6.7 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 80 MPa Show Supplier Material materials with Resistencia a la flexión of 80 MPa | 50%RH | ISO 178 | 2mm/min | |
160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | dry | ISO 179/1eU | |
23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 76 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 76 g/10min | ISO 1133 | 275°C/2.16Kg |
Velocidad de flujo del volumen derretido | 66 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 66 cm³/10min | ISO 1133 | 275°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 25% Mineral Powder | |
Processing methods | Injection Molding |