General
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Densidad | 1.46 g/cm³ Show Supplier Material materials with Densidad of 1.46 g/cm³ | dry | ISO 1183 | ||
Moisture absorption | 23 °C | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | 50%RH | ISO 62 | 2 mm |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2.9 % Show Supplier Material materials with Elongación of 2.9 % | dry | ISO 527-2/1A | 5mm/min | |
5 % Show Supplier Material materials with Elongación of 5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 4.5 GPa Show Supplier Material materials with Módulo de flexión of 4.5 GPa | 50%RH | ISO 178 | 2mm/min | |
7.5 GPa Show Supplier Material materials with Módulo de flexión of 7.5 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 5 GPa Show Supplier Material materials with Módulo elástico of 5 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
7.6 GPa Show Supplier Material materials with Módulo elástico of 7.6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | 50%RH | ISO 178 | 2mm/min | |
190 MPa Show Supplier Material materials with Resistencia a la flexión of 190 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA | |
-30 °C | 3.2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.2 kJ/m² | dry, 50%RH | ISO 179/1eA | ||
23 °C | 3.2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.2 kJ/m² | dry, 50%RH | ISO 179/1eA | ||
23 °C | 6.2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.2 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 37 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 37 kJ/m² | dry | ISO 179/1eU | |
-30 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry, 50%RH | ISO 179/1eU | ||
23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry, 50%RH | ISO 179/1eU | ||
23 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | 50%RH | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 235 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 235 °C | ISO 75/2Af | 1.80 MPa | ||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | 300/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | 300/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, Drinking Water, RoHS 2011/65/UE | |
Color | Black | |
Fillers | 40% Glass Fiber and Mineral Powder | |
Processing methods | Injection Molding |