General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | 2 mm | ISO 62 | 24h immersion at 23°C | ||
Densidad | 1.44 g/cm³ Show Supplier Material materials with Densidad of 1.44 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 1.6 % Show Supplier Material materials with Elongación of 1.6 % | dry | ISO 527-2/1A | 5mm/min | |
1.8 % Show Supplier Material materials with Elongación of 1.8 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 9.5 GPa Show Supplier Material materials with Módulo de flexión of 9.5 GPa | 50%RH | ISO 178 | 2mm/min | |
10.2 GPa Show Supplier Material materials with Módulo de flexión of 10.2 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
11.6 GPa Show Supplier Material materials with Módulo elástico of 11.6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 235 MPa Show Supplier Material materials with Resistencia a la flexión of 235 MPa | 50%RH | ISO 178 | 2mm/min | |
250 MPa Show Supplier Material materials with Resistencia a la flexión of 250 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia a la tracción | 150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 285 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 285 °C | ISO 75/2Af | 1.80 MPa | ||
Temperatura de fusión | 312 °C Show Supplier Material materials with Temperatura de fusión of 312 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | 325/140/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | 325/140/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE, Drinking Water | |
Color | Black | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |