General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 100 % Show Supplier Material materials with Elongación of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elongation at yield | 45 % Show Supplier Material materials with Elongation at yield of 45 % | dry | ISO 527-2/1A | 50mm/min | |
Límite elástico | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | dry | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 0.795 GPa Show Supplier Material materials with Módulo de flexión of 0.795 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 0.82 GPa Show Supplier Material materials with Módulo elástico of 0.82 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 24 MPa Show Supplier Material materials with Resistencia a la flexión of 24 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 195 °C Show Supplier Material materials with Temperatura de fusión of 195 °C | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Plasticizer | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Processing methods | Injection Molding,Profile Extrusion |