General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 2 % Show Supplier Material materials with Absorción de agua of 2 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry, 50%RH | ISO 527-2/1A | min. | 5mm/min | |
Modulus at 50% elongation | 0.024 GPa Show Supplier Material materials with Modulus at 50% elongation of 0.024 GPa | 50%RH | ISO 527-2/1A | ||
0.027 GPa Show Supplier Material materials with Modulus at 50% elongation of 0.027 GPa | dry | ISO 527-2/1A | |||
Módulo al 100 % de elongación | 0.023 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.023 GPa | 50%RH | ISO 527-2/1A | ||
0.028 GPa Show Supplier Material materials with Módulo al 100 % de elongación of 0.028 GPa | dry | ISO 527-2/1A | |||
Módulo de flexión | 0.33 GPa Show Supplier Material materials with Módulo de flexión of 0.33 GPa | 50%RH | ISO 178 | 2mm/min | |
0.48 GPa Show Supplier Material materials with Módulo de flexión of 0.48 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 0.38 GPa Show Supplier Material materials with Módulo elástico of 0.38 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
0.55 GPa Show Supplier Material materials with Módulo elástico of 0.55 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 15 MPa Show Supplier Material materials with Resistencia a la flexión of 15 MPa | 50%RH | ISO 178 | 2mm/min | |
20 MPa Show Supplier Material materials with Resistencia a la flexión of 20 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 55 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 55 kJ/m² | dry | ISO 179/1eA | |
23 °C | 95 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 95 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 110 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 110 kJ/m² | 50%RH | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 50 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 50 °C | ISO 75/2Af | 1.80 MPa |
100 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 100 °C | ISO 75/2Bf | 0.45 MPa | |
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Plasticizer | |
Certifications | RoHS 2011/65/UE | |
Color | Blue | |
Features | Impact Modified, Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |