General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 3.2 % Show Supplier Material materials with Absorción de agua of 3.2 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 65 % Show Supplier Material materials with Elongación of 65 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
100 % Show Supplier Material materials with Elongación of 100 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 4.2 % Show Supplier Material materials with Elongation at yield of 4.2 % | dry | ISO 527-2/1A | 50mm/min | |
10 % Show Supplier Material materials with Elongation at yield of 10 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Límite elástico | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
60 MPa Show Supplier Material materials with Límite elástico of 60 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 1.9 GPa Show Supplier Material materials with Módulo de flexión of 1.9 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 1.4 GPa Show Supplier Material materials with Módulo elástico of 1.4 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 75 MPa Show Supplier Material materials with Resistencia a la flexión of 75 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | 50%RH | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 55 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 55 °C | ISO 75/2Af | 1.80 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 1.6, Class: HB, Standard: UL 94 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Viscosity number | 238 cm³/gr Show Supplier Material materials with Viscosity number of 238 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |