General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 3.2 % Show Supplier Material materials with Absorción de agua of 3.2 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 40 % Show Supplier Material materials with Elongación of 40 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
100 % Show Supplier Material materials with Elongación of 100 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-2/1A | 50mm/min | |
15 % Show Supplier Material materials with Elongation at yield of 15 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Límite elástico | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
70 MPa Show Supplier Material materials with Límite elástico of 70 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 1.3 GPa Show Supplier Material materials with Módulo elástico of 1.3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 750 °C Show Supplier Material materials with Glow Wire Flammability Index of 750 °C | 2 mm | IEC 60695-2-12 | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | 2 mm | IEC 60695-2-13 | ||||
Temperatura de flexión bajo carga | 55 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 55 °C | ISO 75/2Af | 1.80 MPa | ||||
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 185 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 185 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-2, Standard: UL 94 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1 % Show Supplier Material materials with Contracción of 1 % | 270/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.2 % Show Supplier Material materials with Contracción of 1.2 % | 270/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Viscosity number | 146 cm³/gr Show Supplier Material materials with Viscosity number of 146 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Processing methods | Injection Molding |