General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 3 % Show Supplier Material materials with Absorción de agua of 3 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 100 % Show Supplier Material materials with Elongación of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elongation at yield | 15 % Show Supplier Material materials with Elongation at yield of 15 % | dry | ISO 527-2/1A | 50mm/min | |
Límite elástico | 60 MPa Show Supplier Material materials with Límite elástico of 60 MPa | dry | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 80 MPa Show Supplier Material materials with Resistencia a la flexión of 80 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 4.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Viscosity number | 100 cm³/gr Show Supplier Material materials with Viscosity number of 100 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Processing methods | Injection Molding |