General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 2.5 % Show Supplier Material materials with Absorción de agua of 2.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1 % Show Supplier Material materials with Moisture absorption of 1 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 120 % Show Supplier Material materials with Elongación of 120 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-2/1A | 50mm/min | |
Límite elástico | 42 MPa Show Supplier Material materials with Límite elástico of 42 MPa | dry | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 1.4 GPa Show Supplier Material materials with Módulo de flexión of 1.4 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 1.5 GPa Show Supplier Material materials with Módulo elástico of 1.5 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 53 MPa Show Supplier Material materials with Resistencia a la flexión of 53 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 70 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Plasticized Free, Impact Modified, Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |