General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Límite elástico | 65 MPa Show Supplier Material materials with Límite elástico of 65 MPa | dry | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 80 MPa Show Supplier Material materials with Resistencia a la flexión of 80 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 4.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Temperatura de fusión | 213 °C Show Supplier Material materials with Temperatura de fusión of 213 °C | 9.5 mm | ISO 11357-1/-3 | 10°C/min | |||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-2, Standard: UL 94 |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding |