General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.34 g/cm³ Show Supplier Material materials with Densidad of 1.34 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 4.3 % Show Supplier Material materials with Elongación of 4.3 % | dry | ISO 527-2/1A | 5mm/min |
Módulo de flexión | 9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | dry | ISO 178 | 2mm/min |
Módulo elástico | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-2/1A | 1mm/min |
Resistencia a la flexión | 265 MPa Show Supplier Material materials with Resistencia a la flexión of 265 MPa | dry | ISO 178 | 2mm/min |
Resistencia a la tracción | 175 MPa Show Supplier Material materials with Resistencia a la tracción of 175 MPa | dry | ISO 527-2/1A | 5mm/min |
Resistencia al choque, ensayo Charpy no entallado | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | dry | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.7 % Show Supplier Material materials with Contracción of 0.7 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, Drinking Water, RoHS 2011/65/UE | |
Color | Natural | |
Features | Improved Fluiditiy, Hydrolysis Resistance | |
Fillers | 35% Glass Fiber | |
Processing methods | Injection Molding |