General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 5.5 % Show Supplier Material materials with Absorción de agua of 5.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 45 % Show Supplier Material materials with Elongación of 45 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
100 % Show Supplier Material materials with Elongación of 100 % | 50%RH | ISO 527-2/1A | 50mm/min | nominal | ||
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-2/1A | 50mm/min | |
15 % Show Supplier Material materials with Elongation at yield of 15 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Límite elástico | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
55 MPa Show Supplier Material materials with Límite elástico of 55 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 1.3 GPa Show Supplier Material materials with Módulo de flexión of 1.3 GPa | 50%RH | ISO 178 | 2mm/min | |
2.9 GPa Show Supplier Material materials with Módulo de flexión of 2.9 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 1.3 GPa Show Supplier Material materials with Módulo elástico of 1.3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 45 MPa Show Supplier Material materials with Resistencia a la flexión of 45 MPa | 50%RH | ISO 178 | 2mm/min | |
90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 18 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | dry, 50%RH | ISO 179/1eU |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Amorphous, Improved Dimensional Stability, High Surface Aspect, Low moisture absorption, Heat Stabilized | |
Fillers | 10% Mineral Powder | |
Processing methods | Injection Molding |