General
Property | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Absorción de agua | 0.5 % Show Supplier Material materials with Absorción de agua of 0.5 % | 2 mm | ISO 62 | 24h immersion at 23°C | |
Densidad | 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.17 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 3.1 GPa Show Supplier Material materials with Módulo de flexión of 3.1 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 3.6 GPa Show Supplier Material materials with Módulo elástico of 3.6 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 88 MPa Show Supplier Material materials with Resistencia a la tracción of 88 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | dry | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 85 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 85 °C | ISO 75/2Af | 1.80 MPa | ||
Temperatura de fusión | 302 °C Show Supplier Material materials with Temperatura de fusión of 302 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding |