General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 10.9 % Show Supplier Material materials with Absorción de agua of 10.9 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 2.9 % Show Supplier Material materials with Moisture absorption of 2.9 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | |
90 % Show Supplier Material materials with Elongación of 90 % | dry | ISO 527-2/1A | 50mm/min | nominal | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-2/1A | 50mm/min | |
30 % Show Supplier Material materials with Elongation at yield of 30 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Límite elástico | 40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
75 MPa Show Supplier Material materials with Límite elástico of 75 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 0.75 GPa Show Supplier Material materials with Módulo de flexión of 0.75 GPa | 50%RH | ISO 178 | 2mm/min | |
2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 1.1 GPa Show Supplier Material materials with Módulo elástico of 1.1 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 30 MPa Show Supplier Material materials with Resistencia a la flexión of 30 MPa | 50%RH | ISO 178 | 2mm/min | |
100 MPa Show Supplier Material materials with Resistencia a la flexión of 100 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 825 °C Show Supplier Material materials with Glow Wire Flammability Index of 825 °C | 2 mm | IEC 60695-2-12 | ||||
850 °C Show Supplier Material materials with Glow Wire Flammability Index of 850 °C | 1 mm | IEC 60695-2-12 | |||||
Glow Wire Ignition Temperature | 700 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 700 °C | 2 mm | IEC 60695-2-13 | ||||
875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | 1 mm | IEC 60695-2-13 | |||||
Temperatura de flexión bajo carga | 55 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 55 °C | ISO 75/2Af | 1.80 MPa | ||||
170 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 170 °C | ISO 75/2Bf | 0.45 MPa | |||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 195 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 195 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Viscosity number | 190 cm³/gr Show Supplier Material materials with Viscosity number of 190 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Processing methods | Injection Molding,Film Extrusion |