General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.59 g/cm³ Show Supplier Material materials with Densidad of 1.59 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 2.1 % Show Supplier Material materials with Elongación of 2.1 % | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 14.2 GPa Show Supplier Material materials with Módulo de flexión of 14.2 GPa | ISO 178 | 2mm/min | |
Módulo elástico | 12.8 GPa Show Supplier Material materials with Módulo elástico of 12.8 GPa | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 285 MPa Show Supplier Material materials with Resistencia a la flexión of 285 MPa | ISO 178 | 2mm/min | |
Resistencia a la tracción | 190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 54 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 54 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | 23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 11 kJ/m² | ISO 180/1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 260 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 260 °C | ISO 75/2Af | 1.80 MPa | ||
270 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 270 °C | ISO 75/2Bf | 0.45 MPa | |||
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 150 V Show Supplier Material materials with Índice de seguimiento comparativo of 150 V | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | 330/140/50* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | 330/140/50* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Velocidad de flujo de la masa derretida | 40 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 40 g/10min | ISO 1133 | 315°C/5Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Flame Retardant, Impact Modified, Heat Stabilized | |
Fillers | 40% Glass Fiber | |
Processing methods | Injection Molding |