General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 0.3 % Show Supplier Material materials with Absorción de agua of 0.3 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.68 g/cm³ Show Supplier Material materials with Densidad of 1.68 g/cm³ | ISO 1183 | ||||
Moisture absorption | 23 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 8.5 % Show Supplier Material materials with Elongación of 8.5 % | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 2.8 % Show Supplier Material materials with Elongation at yield of 2.8 % | ISO 527-2/1A | 50mm/min | |
Límite elástico | 53 MPa Show Supplier Material materials with Límite elástico of 53 MPa | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 3.6 GPa Show Supplier Material materials with Módulo de flexión of 3.6 GPa | ISO 178 | 2mm/min | |
Módulo elástico | 3.6 GPa Show Supplier Material materials with Módulo elástico of 3.6 GPa | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 85 MPa Show Supplier Material materials with Resistencia a la flexión of 85 MPa | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 37 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 37 kJ/m² | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 20 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 20 g/10min | ISO 1133 | 250°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, RoHS 2011/65/UE | |
Color | Black | |
Features | Metal Detectable | |
Processing methods | Injection Molding |