General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.34 g/cm³ Show Supplier Material materials with Densidad of 1.34 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 3.4 % Show Supplier Material materials with Elongación of 3.4 % | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 4.8 GPa Show Supplier Material materials with Módulo de flexión of 4.8 GPa | ISO 178 | 2mm/min | |
Módulo elástico | 5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 150 MPa Show Supplier Material materials with Resistencia a la flexión of 150 MPa | ISO 178 | 2mm/min | |
Resistencia a la tracción | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 55 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55 kJ/m² | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Temperatura de flexión bajo carga | 145 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 145 °C | ISO 75/2Af | 1.80 MPa | ||||
Temperatura de fusión | 222 °C Show Supplier Material materials with Temperatura de fusión of 222 °C | ISO 11357-1/-3 | 10°C/min | ||||
Inflamabilidad | Thickness tested (mm): 1.6, Class: HB, Standard: UL 94 |
Eléctrico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Velocidad de flujo de la masa derretida | 12 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 12 g/10min | ISO 1133 | 250°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Fillers | 15% Glass Fiber | |
Processing methods | Injection Molding |