General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 10.6 GPa Show Supplier Material materials with Módulo de flexión of 10.6 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 10.8 GPa Show Supplier Material materials with Módulo elástico of 10.8 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 265 MPa Show Supplier Material materials with Resistencia a la flexión of 265 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 168 MPa Show Supplier Material materials with Resistencia a la tracción of 168 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 58 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 58 kJ/m² | dry | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 261 °C Show Supplier Material materials with Temperatura de fusión of 261 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo del volumen derretido | 28 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 28 cm³/10min | ISO 1133 | 275°C/5Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 35% Glass Fiber | |
Processing methods | Injection Molding |