General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 2.9 % Show Supplier Material materials with Elongación of 2.9 % | dry | ISO 527-2/1A | 5mm/min |
Módulo de flexión | 9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | dry | ISO 178 | 2mm/min |
Módulo elástico | 9.4 GPa Show Supplier Material materials with Módulo elástico of 9.4 GPa | dry | ISO 527-2/1A | 1mm/min |
Resistencia a la flexión | 190 MPa Show Supplier Material materials with Resistencia a la flexión of 190 MPa | dry | ISO 178 | 2mm/min |
Resistencia a la tracción | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-2/1A | 5mm/min |
Resistencia al choque, ensayo Charpy no entallado | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 7 kJ/m² | dry | ISO 179/1eU | -30°C |
50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Laser Markable, Flame Retardant, Halogen-free, Phosphorus-free | |
Fillers | 25% Glass Fiber | |
Processing methods | Injection Molding |