General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 8.0 GPa Show Supplier Material materials with Módulo de flexión of 8.0 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 9.3 GPa Show Supplier Material materials with Módulo elástico of 9.3 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 230 MPa Show Supplier Material materials with Resistencia a la flexión of 230 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 8.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8.5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 62 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 62 kJ/m² | dry | ISO 179/1eU | 23°C |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |