General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 10 % Show Supplier Material materials with Elongación of 10 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 4.3 % Show Supplier Material materials with Elongation at yield of 4.3 % | dry | ISO 527-2/1A | 50mm/min | |
Límite elástico | 80 MPa Show Supplier Material materials with Límite elástico of 80 MPa | dry | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 3.0 GPa Show Supplier Material materials with Módulo elástico of 3.0 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 105 MPa Show Supplier Material materials with Resistencia a la flexión of 105 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 4.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.1 % Show Supplier Material materials with Contracción of 1.1 % | 270/60/30* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.2 % Show Supplier Material materials with Contracción of 1.2 % | 270/60/30* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Processing methods | Injection Molding |