General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 20 % Show Supplier Material materials with Elongación of 20 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elongation at yield | 230 % Show Supplier Material materials with Elongation at yield of 230 % | 50%RH | ISO 527-2/1A | 50mm/min | |
Límite elástico | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
65 MPa Show Supplier Material materials with Límite elástico of 65 MPa | dry | ISO 527-2/1A | 50mm/min | ||
Módulo de flexión | 0.72 GPa Show Supplier Material materials with Módulo de flexión of 0.72 GPa | 50%RH | ISO 178 | 2mm/min | |
2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | dry | ISO 178 | 2mm/min | ||
Módulo elástico | 0.85 GPa Show Supplier Material materials with Módulo elástico of 0.85 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 30 MPa Show Supplier Material materials with Resistencia a la flexión of 30 MPa | 50%RH | ISO 178 | 2mm/min | |
100 MPa Show Supplier Material materials with Resistencia a la flexión of 100 MPa | dry | ISO 178 | 2mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 12.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 90 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | dry | ISO 179/1eU |
Aplicaciones térmicas
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.4 % Show Supplier Material materials with Contracción of 1.4 % | 250/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.6 % Show Supplier Material materials with Contracción of 1.6 % | 250/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Velocidad de flujo de la masa derretida | 20 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 20 g/10min | ISO 1133 | 250°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Impact Modified, Heat Stabilized | |
Processing methods | Injection Molding |