General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Límite elástico | 65 MPa Show Supplier Material materials with Límite elástico of 65 MPa | dry | ISO 527-2/1A | 50mm/min | |
Módulo de flexión | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 82 MPa Show Supplier Material materials with Resistencia a la flexión of 82 MPa | dry | ISO 178 | 2mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10.2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10.2 kJ/m² | dry | ISO 179/1eA | |
23 °C | 17 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 17 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Izod entallado | 23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 15 kJ/m² | dry | ISO 180/1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 65 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65 °C | ISO 75/2Af | 1.80 MPa |
190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | ISO 75/2Bf | 5mm | |
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 19 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 19 g/10min | ISO 1133 | 275°C/2.16Kg |
Viscosity number | 140 cm³/gr Show Supplier Material materials with Viscosity number of 140 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Impact Modified | |
Processing methods | Injection Molding |