General
Property | Value |
---|---|
Huella de carbono | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq / T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Medidas
Property | Value |
---|---|
Dimensions | Weight: 7 kg, 10 kg, 16 kg |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 0 - 90 [-] Show Supplier Material materials with Dureza Brinell of 0 - 90 [-] | according to DIN EN 1706 |
Elongación A50 | 23.0 °C | 0 - 8 % Show Supplier Material materials with Elongación A50 of 0 - 8 % | according to DIN EN 1706 |
Límite elástico Rp 0,2 | 23.0 °C | 0 - 220 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 0 - 220 MPa | according to DIN EN 1706 |
Resistencia a la tracción | 23.0 °C | 0 - 320 MPa Show Supplier Material materials with Resistencia a la tracción of 0 - 320 MPa | according to DIN EN 1706 |
Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Hierro | 0 - 0.2 % Show Supplier Material materials with Hierro of 0 - 0.2 % |
Magnesio | 0.15 - 0.6 % Show Supplier Material materials with Magnesio of 0.15 - 0.6 % |
Manganeso | 0.4 - 0.8 % Show Supplier Material materials with Manganeso of 0.4 - 0.8 % |
Otro | 0 - 0.15 % Show Supplier Material materials with Otro of 0 - 0.15 % |
Silicona | 9 - 11.5 % Show Supplier Material materials with Silicona of 9 - 11.5 % |
Titanio | 0 - 0.15 % Show Supplier Material materials with Titanio of 0 - 0.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Structural Applications | |
Processing history | Smelters: Sayanogorsk Aluminium Smelter (SAZ), Khakas Aluminium Smelter (KHAZ), Irkutsk Aluminium Smelter (IrKAZ) |